- 15:26, 26 January 2023 Pevo talk contribs created page Specific Process Knowledge/Thin film deposition/Furnace LPCVD PolySilicon/Boron doped poly-Si (Created page with " ==Results from the acceptance test 2012== {| border="2" cellspacing="1" cellpadding="8" !Recipe name !Deposition rate [nm/min] !Refractive index@630nm !Thickness variation on center wafer !Thickness variation along the boat !Surface roughness [nm] !Sheet resistance [Ohms/square] !Boron concentation [boron atoms/cm<sup>3</sup>] !Comments |- |"DOPEPOLY" |~ 4.0-4.1 (4" wafers) | 1.29%-1.38% (4" wafers) | 1.63%-1.81% (4" wafers) | |~ 4.83, measured with AFM standard tip...")