Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Silicon Oxide/Deposition of Silicon Oxide using PECVD: Difference between revisions

No edit summary
No edit summary
Line 147: Line 147:
|0
|0
|400
|400
|300 LF
|600 LF
|Process for germanium doped core layer developed by Haiyan Ou from DTU Photonics
|Process for germanium doped core layer developed by Haiyan Ou from DTU Photonics
|-
|-
Line 154: Line 154:
|0
|0
|0
|0
|100
|40
|40
|100
|500
|500
|800 LF
|800 LF