Created page with "<i>This page is written by <b>Evgeniy Shkondin @DTU Nanolab</b> if nothing else is stated. <br> All images and photos on this page belongs to <b>DTU Nanolab</b>.<br> The fabrication and characterization described below were conducted in <b>2023</b> by <b>Patama Pholprasit</b> and <b>Evgeniy Shkondin, DTU Nanolab</b>.<br></i> =Evaporation of SiO<sub>2</sub> in Temescal-2= This page describes e-beam evaporation method of SiO<sub>2</sub> in Temescal (10-pocket). E-Beam Ev..."
 
Eves (talk | contribs)
No edit summary
Line 5: Line 5:
=Evaporation of SiO<sub>2</sub> in Temescal-2=
=Evaporation of SiO<sub>2</sub> in Temescal-2=


This page describes e-beam evaporation method of SiO<sub>2</sub> in Temescal (10-pocket). E-Beam Evaporator (10-pockets) - Temescal-2 allows deposition with elevated temperature and O<sub>2</sub> gas bleed. This is ideal conditions of evaporation of oxides such as SiO<sub>2</sub>, TiO<sub>2</sub>, Al<sub>2</sub>O<sub>3</sub> and ITO.
This page describes e-beam evaporation method of SiO<sub>2</sub> in [[Specific Process Knowledge/Thin film deposition/10-pocket e-beam evaporator|10-pocket e-beam evaporator]]. E-Beam Evaporator (10-pockets) - Temescal-2 allows deposition with elevated temperature and O<sub>2</sub> gas bleed. This is ideal conditions of evaporation of oxides such as SiO<sub>2</sub>, TiO<sub>2</sub>, Al<sub>2</sub>O<sub>3</sub> and ITO.


<b>We highly recommend adding 5% O<sub>2</sub> and maintaining a temperature of at least 200&deg;C to achieve high-quality stoichiometric SiO<sub>2</sub> films. Under these conditions, you can expect to produce optical films with smooth surfaces, excellent amorphous properties, and strong adhesion. </b>
<b>We highly recommend adding 5% O<sub>2</sub> and maintaining a temperature of at least 200&deg;C to achieve high-quality stoichiometric SiO<sub>2</sub> films. Under these conditions, you can expect to produce optical films with smooth surfaces, excellent amorphous properties, and strong adhesion. </b>