Specific Process Knowledge/Thermal Process/Oxidation/Breakdown voltage measurements/C3 furnace break-down voltage measurement results: Difference between revisions

From LabAdviser
Pevo (talk | contribs)
Created page with "==Breakdown voltage results for the C3 Anneal-Bond furnace== ===Dry oxidation=== {| border="2" cellspacing="2" cellpadding="5" style="text-align: center;" |- |'''Date''' |'''Oxidation recipe''' |'''Oxide thickness''' |'''Absolute break-down voltage''' |'''Relative break-down voltage''' <i>= Absolute break-down voltage/oxide thickness<i> |- |'''November 2023''' |DRY1100 |488 nm |350x350px|thumb|left |image:..."
 
Pevo (talk | contribs)
 
Line 19: Line 19:
|-
|-
|}
|}
<i>The break-down voltage measurements have been made with help from Kitty Steenberg and Rune Sixten Grass from DTU Health Tech.<i>

Latest revision as of 12:53, 16 September 2025

Breakdown voltage results for the C3 Anneal-Bond furnace

Dry oxidation

Date Oxidation recipe Oxide thickness Absolute break-down voltage Relative break-down voltage

= Absolute break-down voltage/oxide thickness

November 2023 DRY1100 488 nm

The break-down voltage measurements have been made with help from Kitty Steenberg and Rune Sixten Grass from DTU Health Tech.