Breakdown voltage results for the A3 Phosphorus Drive-in furnace
Dry oxidation
Wet oxidation
| Date | Oxidation recipe | Oxide thickness | Absolute break-down voltage | Relative break-down voltage
= Absolute break-down voltage/oxide thickness |
| November 2021 | WET1050 | ~320 nm | ||
| January 2024 | WET1050 | ~308 nm |
The break-down voltage measurements have been made with help from Kitty Steenberg and Rune Sixten Grass from DTU Health Tech.