Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/Lasers sources
Appearance
Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.
Laser sources
The laser micromachining tool is equipped with a tunable laser sources from 211 fs to 10 ps. The technical specifications provided by the supplier 3D micromac are shown below. Refer to the Performances to know the measured values of the output power. \ rkch.
Specifications from 3D micromac
| Picosecond (TBW) | ||
| Wavelength | 1030nm, 515nm, 343nm | |
| Pulse duration | 211fs to 10ps software controlled | |
| Repetition rate | 200 kHz up to 8000 kHz software controlled | |
| Output power | 40 W @ 1030 nm | |
| Warm-up time | 25min |