Main public logs
Appearance
Combined display of all available logs of LabAdviser. You can narrow down the view by selecting a log type, the username (case-sensitive), or the affected page (also case-sensitive).
- 11:03, 27 January 2020 Choi talk contribs uploaded File:FumehoodOverview.png (Overview of fume hoods in cleanroom. Updated January 2020.)
- 14:33, 26 November 2018 Choi talk contribs uploaded File:CurrentProfiles2019.png (Standard processes on 2.017 Electroplating-Ni)
- 11:27, 19 October 2018 Choi talk contribs uploaded File:Dscplot.png (Phase transitions in DSC analysis)
- 13:39, 18 October 2018 Choi talk contribs uploaded File:DSCPE.jpg (Picture of DSC Perkin Elmer in PackLab)
- 10:40, 8 May 2018 Choi talk contribs uploaded File:Electroplater-D3.jpg (2.017 Electroplating-Ni i D-3)
- 12:49, 12 February 2018 Choi talk contribs uploaded File:14b-micrograph.png
- 12:49, 12 February 2018 Choi talk contribs uploaded File:13-cycleanalysis.png
- 11:30, 12 February 2018 Choi talk contribs uploaded File:14-micrograph.png
- 11:30, 12 February 2018 Choi talk contribs uploaded File:13-cycletime.png
- 14:19, 9 February 2018 Choi talk contribs uploaded File:12-nozzlemove.png
- 14:05, 8 February 2018 Choi talk contribs uploaded File:11-grid.png
- 14:05, 8 February 2018 Choi talk contribs uploaded File:10-deposit.png
- 12:53, 8 February 2018 Choi talk contribs uploaded a new version of File:07a-eject.png (Ejector pin settings 1)
- 12:52, 8 February 2018 Choi talk contribs uploaded File:07b-eject.png (Ejector pin settings 2)
- 12:51, 8 February 2018 Choi talk contribs uploaded File:07a-eject.png (Ejector pin settings 1)
- 15:17, 25 January 2018 Choi talk contribs uploaded File:09-tower.png
- 15:16, 25 January 2018 Choi talk contribs uploaded File:07-eject.png
- 15:16, 25 January 2018 Choi talk contribs uploaded File:08 robot.png
- 15:16, 25 January 2018 Choi talk contribs uploaded File:06-demold.png
- 15:16, 25 January 2018 Choi talk contribs uploaded File:05-dosing.png
- 15:16, 25 January 2018 Choi talk contribs uploaded File:04-holding.png
- 15:15, 25 January 2018 Choi talk contribs uploaded File:03-switchover.png
- 15:15, 25 January 2018 Choi talk contribs uploaded File:02-inject.png
- 15:15, 25 January 2018 Choi talk contribs uploaded File:01-moldclose.png
- 10:59, 24 January 2018 Choi talk contribs uploaded File:Currentprofilestep2018.png (Graph showing Danchip electroplating standard programs.)
- 14:54, 19 January 2018 Choi talk contribs uploaded File:InnovaHardness.jpg (Picture of Innovatest hardness tester)
- 13:43, 27 October 2017 Choi talk contribs uploaded File:Cleanroom naming 2017.jpg (Map of the cleanroom. Updated 25-07-2017.)
- 09:26, 22 September 2017 Choi talk contribs uploaded File:RCA-HF.jpg (HF baths in RCA wet bench in cleanroom B1.)
- 09:15, 22 September 2017 Choi talk contribs uploaded File:WB05.jpg (Wet bench 05 in cleanroom D-3.)
- 09:15, 22 September 2017 Choi talk contribs uploaded File:WB03.jpg (Wet bench 03 in cleanboom D-3.)
- 09:14, 22 September 2017 Choi talk contribs uploaded File:WaferClean.jpg (Wafer cleaning bath in wet bench 03)
- 09:13, 22 September 2017 Choi talk contribs uploaded File:MaskClean.jpg (Mask cleaning bath in wet bench 03.)
- 09:13, 22 September 2017 Choi talk contribs uploaded File:FH07.jpg (Fume hood 07 in cleanroom D-3.)
- 09:12, 22 September 2017 Choi talk contribs uploaded File:FH01-02.jpg (Fume hood 01 and 02 in cleanroom D-3.)
- 09:12, 22 September 2017 Choi talk contribs uploaded File:AlEtch.jpg (Aluminium etch in wet bench 05.)
- 09:52, 27 February 2017 Choi talk contribs uploaded File:Fumehood1-2.jpg (Photo of Fumehood 1 and 2 in cleanroom D-3.)
- 11:43, 14 December 2015 Choi talk contribs uploaded File:Currentprofilestep2.png (Current profiles for Danchip standard programs on Electroplating-Ni)
- 11:09, 13 June 2013 Choi talk contribs uploaded File:1042 spraycoater overview.jpg (Overview picture of spray coater)
- 15:42, 27 May 2013 Choi talk contribs uploaded File:Choi 2017 current profiles.jpg (Current profiles showing the first two hours of Danchip's standard programs for making nickel shims for the polymer injection molding machine.)
- 14:29, 7 May 2013 Choi talk contribs uploaded File:Choi 2017 Machine overview.jpg
- 14:51, 7 March 2011 Choi talk contribs uploaded File:Imm.jpg (Picture of the IMM.)