File:RIE1 150nitride bgenitr 3.5min.tif
Appearance
Size of this preview: 800 × 600 pixels. Other resolution: 1,024 × 768 pixels.
Original file (1,024 × 768 pixels, file size: 71 KB, MIME type: image/jpeg)
RIE1 etch profile - 150 nm silicon nitride - recipe "BGE_NITR" (pressure 42 mTorr) - etchtime 3,5 min. The structures are made with e-beam lithography, and the Al etch mask has been removed. Wafer tiltet 45 degrees.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 11:35, 21 September 2009 | 1,024 × 768 (71 KB) | Pvl (talk | contribs) | RIE1 etch profile - 150 nm silicon nitride - recipe "BGE_NITR" (pressure 42 mTorr) - etchtime 3,5 min. The structures are made with e-beam lithography, and the Al etch mask has been removed. Wafer tiltet 45 degrees. | |
| 11:24, 21 September 2009 | 1,024 × 768 (71 KB) | Pvl (talk | contribs) | RIE1 etch profile - 150 nm silicon nitride - recipe "BGE_NITR" (pressure 42 mTorr) - etchtime 3,5 min. The structures are made with e-beam lithography, and the Al etch mask has been removed. Wafer tiltet 45 degrees. | ||
| 11:17, 21 September 2009 | No thumbnail | 1,024 × 768 (769 KB) | Pvl (talk | contribs) | RIE1 etch profile - 150 nm silicon nitride - recipe "BGE_NITR" (pressure 42 mTorr) - etchtime 3,5 min. The structures are made with e-beam lithography, and the Al etch mask has been removed. Wafer tiltet 45 degrees. | |
| 16:03, 7 September 2009 | No thumbnail | 1,024 × 768 (769 KB) | Pvl (talk | contribs) | RIE1 etch profile - 150 nm silicon nitride - recipe "BGE_NITR" (pressure 42 mTorr) - etchtime 3,5 min. The structures are made with e-beam lithography, and the Al etch mask has been removed. Wafer tiltet 45 degrees. |