File:KOH Anisotropy(110).jpg
Appearance
KOH_Anisotropy(110).jpg (465 × 156 pixels, file size: 26 KB, MIME type: image/jpeg)
Sketch of Si(110)-anisotropy
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 11:55, 28 February 2008 | 465 × 156 (26 KB) | Fj (talk | contribs) | Sketch of anisotropy in Si(110) | |
| 17:11, 27 February 2008 | 465 × 156 (28 KB) | Fj (talk | contribs) | Sketch of Si(110)-anisotropy |