File:Hossein-ARGUS-Topography.jpg
Appearance
Size of this preview: 695 × 600 pixels. Other resolution: 1,024 × 884 pixels.
Original file (1,024 × 884 pixels, file size: 1.4 MB, MIME type: image/jpeg)
ARGUS image of martensitic steel. Image is obtained using the following settings: Accelerating voltage: 15 kv Probe current: 3.9 nA ARGUS detector, 9 degrees tilted and 17 mm away from the sample