AFM picture of Cr layer sputter deposited in Wordentec. Settings: 405W, 0.004mbar
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 10:14, 13 August 2008 | 795 × 628 (97 KB) | Kn (talk | contribs) | AFM picture of Cr layer sputter deposited in Wordentec. Settings: 405W, 0.004mbar |