File:Boron concentration2.jpg
Appearance
Size of this preview: 800 × 565 pixels. Other resolution: 1,000 × 706 pixels.
Original file (1,000 × 706 pixels, file size: 65 KB, MIME type: image/jpeg)
Boron doped poly vary B2H6 from 3 sccm to 40 sccm Zoom in
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 14:55, 13 October 2015 | 1,000 × 706 (65 KB) | Paphol (talk | contribs) | Boron doped poly vary B2H6 from 3 sccm to 40 sccm Zoom in |
You cannot overwrite this file.
File usage