File:BGE Glass etch Lesker test2 pinholes 4.jpg
Appearance
Size of this preview: 800 × 600 pixels. Other resolution: 2,560 × 1,920 pixels.
Original file (2,560 × 1,920 pixels, file size: 148 KB, MIME type: image/jpeg)
Borofloat etch with silicon mask made in the Lesker at 200dg. Resist mask from the pattering is on and has been heated to 180 degrees before etching in 40% HF for 15 min.