Borofloat etch with silicon mask made in the Lesker at 200dg. Resist mask from the pattering has been removed before etching in 40% HF for 15 min.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current17:00, 1 December 2010Thumbnail for version as of 17:00, 1 December 20102,560 × 1,920 (159 KB)BGE (talk | contribs)Borofloat etch with silicon mask made in the Lesker at 200dg. Resist mask from the pattering has been removed before etching in 40% HF for 15 min.