File:BGE Glass etch Cr50Au400n1 pinholes 01.jpg
Appearance
Size of this preview: 800 × 600 pixels. Other resolution: 2,560 × 1,920 pixels.
Original file (2,560 × 1,920 pixels, file size: 223 KB, MIME type: image/jpeg)
15min HF 40% etch of borofloat with 50/400 nm Cr/Au mask made in the Alcatel E-beam evaporator. Resist for masking the Cr/Au etch has been left on and baked at 120 degrees of ½ hour. The image is taken where I found some pinholes.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 10:10, 3 December 2010 | 2,560 × 1,920 (223 KB) | BGE (talk | contribs) | 15min HF 40% etch of borofloat with 50/400 nm Cr/Au mask made in the Alcatel E-beam evaporator. Resist for masking the Cr/Au etch has been left on and baked at 120 degrees of ½ hour. The image is taken where I found some pinholes. |