File:Amor540 24Hours.png
Appearance
Size of this preview: 800 × 381 pixels. Other resolution: 930 × 443 pixels.
Original file (930 × 443 pixels, file size: 335 KB, MIME type: image/png)
LPCVD Poly furnace Recipe: Amor540, deposition time 24hours, film thickness 2um.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 11:38, 4 June 2020 | 930 × 443 (335 KB) | Paphol (talk | contribs) | LPCVD Poly furnace Recipe: Amor540, deposition time 24hours, film thickness 2um. |
You cannot overwrite this file.
File usage
The following 2 pages use this file: