File:AFMpict Cu Alc 10Å S.jpg
Appearance
Size of this preview: 759 × 600 pixels. Other resolution: 795 × 628 pixels.
Original file (795 × 628 pixels, file size: 94 KB, MIME type: image/jpeg)
AFM picture of a Cu layer deposited in Alcatel. Dep. rate 10 Å/s.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 16:32, 16 December 2008 | 795 × 628 (94 KB) | Kn (talk | contribs) | AFM picture of a Cu layer deposited in Alcatel. Dep. rate 10 Å/s. |
You cannot overwrite this file.
File usage
The following file is a duplicate of this file (more details):
There are no pages that use this file.