File:A3 furnace 100 Si wet oxidation.jpg
Appearance
A3_furnace_100_Si_wet_oxidation.jpg (706 × 443 pixels, file size: 129 KB, MIME type: image/jpeg)
Oxidation curve for Si-<100> wet oxidation in furnace A3