- 11:11, 5 November 2026 Cchvi talk contribs created page Specific Process Knowledge/Polymer Processing/PDMS Post-processing (Created page with " The fabrication of microfluidic devices requires further processing of PDMS, including cutting, creating through-holes, bonding to other parts, and surface functionalization. 1000px|frame|center|Fabrication of microfluidic device by casting of PDMS on SU-8/silicon mould, folowed by punching of through holes, and glass, vial bonding ==Cutting of PDMS== Cutting of PDMS is a common step in the fabrication of PDMS microfluidics to create...")