  • 10:41, 12 January 2026 Jehem talk contribs created page Specific Process Knowledge/Lithography/Resist/UVresist/exposureDoseMaskAligners (Created page with "==Exposure dose for mask aligners== The exposure doses listed below are for ''generic'' good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values. All doses are for standard silicon wafers, unless otherwise stated. Development is done using 2.38% TMAH (AZ 726 MIF). ===Aligner: MA6-1=== The Align...")