- 14:47, 15 March 2011 Jml talk contribs uploaded File:WF 2B4 feb06 2011-030.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.3 recipe, Run ID 430 and 432, time 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 20 degs.)