Jump to content

Specific Process Knowledge/Characterization/KLA-Tencor Surfscan 6420

From LabAdviser

Feedback to this page: click here

KLA-Tencor Surfscan 6420

 
The image is from the cleanroom at the place it was refurbish in California.

Particle counting of an unpatterned surface. A broad range of particles size from 0.15 µm to greater than 3 µm can be measured on a polished silicon or epitaxial layers. Thin films like Nitride and thermal Oxide can also be inspected. The system will remove small surface roughness so it will not count as particles.



Overview of the performance of the Surfscan 6420 and some process related parameters

Purpose
  • Particles counting
Performance Particles size
  • 0.1 µm to 3 µm
Througput
  • Up to 100 wafer per hour (200 mm)
Repeatbility
  • Within 1%, 1σ (mean count > 500, 0,204 µm diameter latex spheres)
Process parameter range Process Temperature
  • Room temperature
Process pressure
  • 1 atm
Substrates Batch size
  • Small wafer pieces can all be used
  • 1-25 100 mm wafers
  • 1-25 150 mm wafers
  • 1-25 200 mm wafers
Substrate material allowed