Comparing silicon nitride etch methods at Danchip
Feedback to this page: click here
Comparing silicon nitride etch methods at Danchip ![Section under construction.jpg](/images/thumb/9/9a/Section_under_construction.jpg/70px-Section_under_construction.jpg)
There are a broad varity of silicon nitride etch methods at Danchip. The methodes are compared here to make it easier for you to compare and choose the one that suits your needs.
- Wet Silicon Nitride Etch
- Etch of Silicon Nitride using RIE
- Etch of Silicon Nitride using AOE
- IBE/Ion Beam Etching using IBSD Ionfab 300
Compare the methods for Silicon Nitride etching
Wet Silicon Nitride Etch | BHF | RIE (Reactive Ion Etch) | AOE (Advanced Oxide Etch) | IBE/IBSD Ionfab 300 | |
---|---|---|---|---|---|
Generel description |
|
|
|
|
|
Possible masking materials |
|
|
|
|
|
Etch rate range |
|
|
|
|
|
Substrate size |
|
|
|
|
|
Allowed materials |
|
|
|
|
|