The BCB Curing Oven is mainly used for curing of BCB (bisbenzocyclobutene) and for alloying of metal in a nitrogen atmosphere.
During processing the furnace is rapidly heated by use of five halogen lamps below the sample. The furnace is purged with a high or a low nitrogen flow. Samples are processed at atmospheric pressure or at vacuum
The user manual, user APV, technical information and contact information can be found in LabManager:

Process information
There are no standard processes on the furnace.
Equipment | BCB Curing Oven | |
---|---|---|
Purpose |
| |
Process parameter range | Temperature |
|
Nitrogen flows |
| |
Substrates | Batch size |
|
Allowed materials
Use the right carrier wafer |
|