Specific Process Knowledge/Thermal Process/C1 Furnace Anneal-oxide
Appearance
C1 Furnace Anneal Oxide
C1 Furnace Anneal Oxide is a Tempress horizontal furnace for oxidation and annealing of silicon wafers. The furnace is the only one there can handel 6" wafer.
This furnace is the first furnace tube in the furnace C-stack positioned in cleanroom 2. In this furnace it is allowed to enter wafers that comes directly from PECVD1 (assuming they were very clean when entering PECVD1). Check the cross contamination chart. If you are in doubt, please send a mail to furnace@danchip.dtu.dk.
The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:
Process knowledge
| Purpose | Oxidation and annealing | Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|