File:W5 center.JPG
Appearance
Size of this preview: 651 × 600 pixels. Other resolution: 1,024 × 943 pixels.
Original file (1,024 × 943 pixels, file size: 200 KB, MIME type: image/jpeg)
CNTs, wafer 5. Recipe "PECVD NH3.txt" 5 min growth.