Specific Process Knowledge/Thin film deposition/Deposition of Copper
Copper can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | Sputter deposition (PVD co-sputter/evaporation) | |
---|---|---|
Batch size |
|
|
Pre-clean | RF Ar clean | RF Ar clean |
Layer thickness | 10Å to 0.5µm |
10Å to 0.5µm |
Deposition rate | 2Å/s to 15Å/s |
Depending on process paraneters |
Studies of Cu deposition processes
Roughness of Cu layers - Roughness of Cu layers deposited with Alcatel