Copper can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Alcatel) | Sputter deposition (PVD co-sputter/evaporation) | |
|---|---|---|
| Batch size |
|
.. |
| Pre-clean | RF Ar clean |
.. |
| Layer thickness | 10Å to 0.5µm |
.. |
| Deposition rate | 2Å/s to 15Å/s |
.. |
Studies of Cu deposition processes
Roughness of Cu layers - Roughness of Cu layers deposited with Alcatel