Specific Process Knowledge/Etch/Etching of Silicon
Appearance
Etch of silicon can be done by either wet etch or dry etch. The standard setups for this here at DANCHIP are:
Wet etches:
Dry etches:
Comparison of KOH etch, wet PolySilicon etch, RIE etch and ASE etch for etching of Silicon
| KOH | PolySilicon etch | RIE | ASE | |
|---|---|---|---|---|
| What is it good for: |
|
|
|
|
| Possible masking materials: |
|
|
|
|
| Etch rate |
|
|
<40nm/min to >600nm/min depending on recipe parameters and mask design | <130nm/min to >5.6 µm/min depending on recipe, mask design and aspect ratio. |
| Size of substrate | 4" and 6" in our standard bath | 4" in our standard bath | 4" (or smaller with carrier) | 6" (when it is set up for 6") and 4" (or smaller if you have a carrier) |
| Process volume | 25 wafers at a time | 25 wafers at a time | One wafer at a time | One wafer at a time |