File:PMMA plasma treatment.png

From LabAdviser
Revision as of 10:46, 5 November 2026 by Cchvi (talk | contribs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,181 × 281 pixels, file size: 125 KB, MIME type: image/png)

Surface activation of PMMA after oxygen plasma treatment, contact angle of water

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current10:46, 5 November 2026Thumbnail for version as of 10:46, 5 November 20261,181 × 281 (125 KB)Cchvi (talk | contribs)

Metadata