Inkjet printer

Inkjet printer is located in PolyFabLab, building 347.
Inkjet printer is located in PolyFabLab, building 347.

The inkjet printer is an Autodrop Gantry II printing system bought in 2020 and installed in PolyFabLab in 2025. It is a modular XYZ positioning platform for contact-less, piezo-driven inkjet dispensing. It drives interchangeable dispenser heads, Autopipettes, or piezo valves rather than a single fixed printhead, and is intended for precision deposition of inks, polymers, and other functional fluids on chips, wafers, and other flat substrates — for process development, prototyping, and small-batch work rather than high-throughput production.

The user manual and contact information for the inkjet printer can be found on LabManager LabManager - requires login


Equipment performance and process-related parameters

Purpose Contactless, drop-on-demand deposition of inks/fluids for materials and pattern printing
Working principle Piezo-driven drop-on-demand (DOD) inkjet
Dispensing volume Picoliter to microliter per drop, head-dependent
Nozzle diameter 30–80 µm, head-dependent
Number of heads Up to 4x dispenser heads, Autopipettes, or piezo valves
Travel range 300 mm x 300 mm x 100 mm (X/Y/Z), scalable
Positioning accuracy ±20 µm
Repetition accuracy ±5 µm
Substrate handling Vacuum table/holder — free choice of assembly
Substrate batch 1 (single substrate per run, standard configuration)