Original file (2,738 × 1,365 pixels, file size: 90 KB, MIME type: image/png)

Graphs of contact angle for water on PDMS and borosilicate glass vs oxygen plasma treatment time

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current16:32, 16 July 2026Thumbnail for version as of 16:32, 16 July 20262,738 × 1,365 (90 KB)Cchvi (talk | contribs)