Revision as of 12:17, 12 January 2026 by Jehem (talk | contribs) (Created page with "=Plasma Asher 3: Descum= 400px|thumb|Plasma Asher 3: Descum is a low power plasma asher dedicated for descumming on smaller substrates. Product name: Diener Pico Plasma Asher<br> Year of purchase: 2014 The Plasma Asher 3: Descum is dedicated for resist descum, i.e. removal of remains resist traces after development. It has a small chamber, so you can only load a single 100 mm substrate, or a few smaller pieces. In this machine, only Ox...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Plasma Asher 3: Descum

 
Plasma Asher 3: Descum is a low power plasma asher dedicated for descumming on smaller substrates.

Product name: Diener Pico Plasma Asher
Year of purchase: 2014

The Plasma Asher 3: Descum is dedicated for resist descum, i.e. removal of remains resist traces after development. It has a small chamber, so you can only load a single 100 mm substrate, or a few smaller pieces.

In this machine, only Oxygen is used for processing.

Typical process parameters:
Process: Photoresist descumming
Pressure: 0.2-0.8 mbar
Gas: 45 sccm O2
Power: 100 W (100%)
Time: 1 -10 minutes (depending on photoresist type and thickness)

Other materials have not been tested.

The user manual, user APV, and contact information can be found in LabManager - requires login

Process Information

Detailed information about descum processing on Plasma asher 3: Descum can be found here.