TPT HB100 wire bonder comes with wires and tools and has option for mounting Gold wire (dia.: 25µm) or Aluminum wire (dia.: 33µm). write to the tool responsible person for changing wire. The system has motorized Z-Y-X Axes and Bond Head Rotation. The TPT software has template of recipes allowing user to set up their own process recipe based on type of bonding and wire.
Table: HB100 Full Technical Specifications
| Bonding Specifications | Bonding Methods | Wedge–Wedge, Ball–Wedge, Ribbon, Bump |
|---|---|---|
| Bond Head Capability | One head for Wedge & Ball bonding (tool change only) | |
| Wire Diameter (Gold) | 12–75 µm (0.5–3 mil) | |
| Wire Diameter (Aluminium) | 17–75 µm (0.7–3 mil) | |
| Wire & Ribbon Handling | Ribbon Size | Max. 25 × 250 µm (1 × 10 mil) |
| Wire Spool Size | 2" diameter | |
| Wire Feed Angle / Immersion Depth | 90° deep access / 14 mm immersion | |
| Ultrasonic & Bonding Parameters | Ultrasonic Frequency | 63.3 kHz PLL control (110 kHz option) |
| Ultrasonic Power | 0–10 W | |
| Bond Time | 0–5 seconds | |
| Bond Force | 10–200 cN | |
| Bonding Tool Size | 1.58 mm Ø × 19 mm length (0.0624” × 0.750”) | |
| Wire Termination | Bond Head Tear or Clamp Tear | |
| Mechanics & Motion Control | Z-Drive / Resolution | Lead screw motor / 0.5 µm |
| Motorized Z Travel | 100 mm (3.9”) | |
| X–Y Drive / Resolution | Linear motors / 0.1 µm | |
| Motorized X–Y Travel | 100 mm (3.9”) | |
| Max. Component Width | 400 mm (15.7”) | |
| Rotation Drive Accuracy | ±0.5° | |
| Control & Interface | Axis Control | Joystick |
| Screen Size | 21” touchscreen | |
| Software Environment | Industrial PC with Windows | |
| Camera & Optics | Camera System | Dual camera (detail + overview) |
| Magnification | Up to 150× | |
| View Mode | Simultaneous detail & overview | |
| Heater Stage | Size | 90 mm Ø surface (mechanical & vacuum clamping) |
| Temperature Range | Up to 200 °C ±1 °C | |
| Clamping | Mechanical & vacuum |