Specific Process Knowledge/Thin film deposition/Deposition of Niobium Nitride
Appearance
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Deposition of Niobium Nitride
Deposition of ScN can only be done by reactive sputtering using Nb target.
The primary tool for this application is the Cluster-Based, multi-chamber high-vacuum sputtering deposition system, commonly referred to as the 'Cluster Lesker.' The operating process is thoroughly documented and described in detail.:
- Deposition of Niobium Nitride (NbN) using reactive p-DC sputtering in Sputter-System Metal-Nitride(PC3) Source 2 (3-inch target)
At the moment (July 2025) we have a 3-inch Nb target (0.250" thick) for PC1 and PC3.