Deposition of MoSi using sputtering method

Molybdenum silicide is particularly attractive for optical coatings because co-sputtering Mo with Si allows precise control of MoSi stoichiometry—and, in turn, the film’s refractive index at the design wavelength.

MoSi alloy can be deposited by DC co-sputtering in either Sputter-System Metal-Oxide(PC1) or Sputter-System Metal-Nitride (PC3)—collectively referred to as the Cluster Lesker. The process uses two 3-inch targets:

  • Mo (unbonded)
  • Si (indium-bonded)

Achieving the desired composition and optical properties requires careful tuning of three key parameters:

  • Magnetron power on each target
  • Substrate temperature
  • Deposition pressure

Below is a link summarizing process results obtained with the Metal-Oxide (PC1) system: