The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.

Feedback to this page: click here


Removal of native oxide is a part of the RCA cleaning procedure. See the RCA page for further details. The HF/BHF baths in the RCA bench bath must only be used during the RCA cleaning procedure. For removal of oxide of processed wafers that is not getting a full RCA clean the other HF/BHF baths can be used. Please see the oxide etch page for more details.