File:WF 2E09b mar23 2011-120.jpg
Appearance
Size of this preview: 800 × 600 pixels. Other resolution: 1,024 × 768 pixels.
Original file (1,024 × 768 pixels, file size: 328 KB, MIME type: image/jpeg)
Etching of nanostructures in Si using ASE: pxnano2 recipe, time 96 secs (12 cycles), temp 20 degrees
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 12:24, 19 May 2011 | 1,024 × 768 (328 KB) | Jml (talk | contribs) | Etching of nanostructures in Si using ASE: pxnano2 recipe, time 96 secs (12 cycles), temp 20 degrees |