Revision as of 12:24, 19 May 2011 by Jml (talk | contribs) (Etching of nanostructures in Si using ASE: pxnano2 recipe, time 96 secs (12 cycles), temp 20 degrees)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 768 pixels, file size: 344 KB, MIME type: image/jpeg)

Etching of nanostructures in Si using ASE: pxnano2 recipe, time 96 secs (12 cycles), temp 20 degrees

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current12:24, 19 May 2011Thumbnail for version as of 12:24, 19 May 20111,024 × 768 (344 KB)Jml (talk | contribs)Etching of nanostructures in Si using ASE: pxnano2 recipe, time 96 secs (12 cycles), temp 20 degrees