Jump to content

File:25W - thickness PECVD4 nitride QC.png

From LabAdviser
Revision as of 14:46, 4 March 2025 by Mfarin (talk | contribs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

25W_-_thickness_PECVD4_nitride_QC.png (751 × 465 pixels, file size: 9 KB, MIME type: image/png)

tests from november to february of 25W QC nitride, date vs tickness

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current14:46, 4 March 2025Thumbnail for version as of 14:46, 4 March 2025751 × 465 (9 KB)Mfarin (talk | contribs)