Revision as of 08:29, 9 May 2011 by Jml (talk | contribs) (Etching of nanostructures in Si using DRIE-Pegasus: nano1.42 recipe, Run ID 2017, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/40 coil/platen, -20 degs.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 768 pixels, file size: 122 KB, MIME type: image/jpeg)

Etching of nanostructures in Si using DRIE-Pegasus: nano1.42 recipe, Run ID 2017, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/40 coil/platen, -20 degs.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current08:29, 9 May 2011Thumbnail for version as of 08:29, 9 May 20111,024 × 768 (122 KB)Jml (talk | contribs)Etching of nanostructures in Si using DRIE-Pegasus: nano1.42 recipe, Run ID 2017, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/40 coil/platen, -20 degs.