Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current12:42, 29 April 2011Thumbnail for version as of 12:42, 29 April 20111,024 × 768 (133 KB)Jml (talk | contribs)Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs.
12:40, 29 April 2011Thumbnail for version as of 12:40, 29 April 20111,024 × 768 (93 KB)Jml (talk | contribs)Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs.

Metadata