The DREM processes

DREM 2kW micro

DREM 2kW micro
Recipe General Pressure Gases Generators Matching Results
C4F8 SF6 Coil Platen Coil Platen
T S/E Dp D B M D B M D B M Dp Dep L T L T Pressure Runs
H/L Cyc Et D B M D B M D B M Et D B M L T L T Keywords
DREM 2kW micro Pump to base, Clamp Substrate, home platen matching unit, stabilisation 8
0 D/E 1.2 100% 0.3@5 0.5@ 50 200 0.3@ 200 0.5@ 200 15 2 1 40 50 32.5 51.9
HF 3 100% 0.5@ 100 5 2@ 15 0.3@ 100 200 2 1@1 1@ 100 1 40 50 32.5 51.9
DREM 2kW micro Pump to base, Clamp Substrate, home platen matching unit, stabilisation 1
-19 D/E 1.2 100% 0.3 @5 0.5@ 50 200 0.3@ 200 0.5@ 200 15 2 1 40 50 32.5 51.9
HF 3 100% 0.5@ 100 5 2@ 15 0.3@ 100 200 2 1@1 1@ 100 1 40 50 32.5 51.9