Specific Process Knowledge/Etch/DRIE-Pegasus/nanoetch
Appearance
| Recipe | nano1.0 | nano1.1 | nano1.2 | nano1.3 | nano1.21 |
|---|---|---|---|---|---|
| C4F8 (sccm) | 52 | 52 | 52 | 52 | 75 |
| SF6 (sccm) | 38 | 38 | 38 | 38 | 38 |
| O2 (sccm) | 0 | 0 | 0 | 0 | 0 |
| Coil power (W) | 800 (forward) | 600 (forward) | 800 (forward) | 600 (forward) | 800 (forward) |
| Platen power (W) | 50 | 50 | 50 | 40 | 50 |
| Pressure (mtorr) | 4 | 4 | 4 | 4 | 4 |
| Temperature (degs C) | 10 | 10 | -10 | -10 | -10 |
| Process time (s) | 120 | 120 | 120 | 120 | 120 |
| Nominal line width | Etched depths (nm) | ||||
| 30 nm | |||||
| 60 nm | |||||
| 90 nm | |||||
| 120 nm | |||||
| 150 nm | |||||
| Nominal line width | Etch rates in trenches (nm/min) | ||||
| 30 nm | |||||
| 60 nm | |||||
| 90 nm | |||||
| 120 nm | |||||
| 150 nm | |||||
| Etch rates in zep resist (nm/min) | |||||
| One point on wafer | |||||
| Images | Images | Images | Images | Images | Images |
The nanoetch