Nano scale etching of silicon nitride with SF6 plasma

Based on silicon etch recipe made by Henri Jansen

silicon nitride etch
Parameter Silicon nitride etch, platen only
SF6 (sccm) 5
Pressure (mTorr) 5
Platen power (W) 20
Temperature (oC) 20