File:WF 2E05 mar23 2011-060b.jpg

From LabAdviser
Revision as of 14:20, 7 April 2011 by Jml (talk | contribs) (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.32 recipe, Run ID 465, 466 and 467, time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/30 coil/platen, 50 degs. 100 mm spacers)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 768 pixels, file size: 110 KB, MIME type: image/jpeg)

Etching of nanostructures in Si using the ICP metal etcher: Sinano3.32 recipe, Run ID 465, 466 and 467, time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/30 coil/platen, 50 degs. 100 mm spacers

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current14:20, 7 April 2011Thumbnail for version as of 14:20, 7 April 20111,024 × 768 (110 KB)Jml (talk | contribs)Etching of nanostructures in Si using the ICP metal etcher: Sinano3.32 recipe, Run ID 465, 466 and 467, time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/30 coil/platen, 50 degs. 100 mm spacers

Metadata