Revision as of 14:17, 7 April 2011 by Jml (talk | contribs) (The profiles of the 211 nm thick zep resist wafers (The E-batch of march 23 2011). The wafers have been over-exposed in the E-beam (400 µC/cm2) to make sure that all structures are opened - therefore the 30, 60, 90, 120 and 150 nm lines are somewhat wide)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 768 pixels, file size: 114 KB, MIME type: image/jpeg)

The profiles of the 211 nm thick zep resist wafers (The E-batch of march 23 2011). The wafers have been over-exposed in the E-beam (400 µC/cm2) to make sure that all structures are opened - therefore the 30, 60, 90, 120 and 150 nm lines are somewhat wider.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current14:17, 7 April 2011Thumbnail for version as of 14:17, 7 April 20111,024 × 768 (114 KB)Jml (talk | contribs)The profiles of the 211 nm thick zep resist wafers (The E-batch of march 23 2011). The wafers have been over-exposed in the E-beam (400 µC/cm2) to make sure that all structures are opened - therefore the 30, 60, 90, 120 and 150 nm lines are somewhat wide