Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 452(abc), 453(bc) and 454 (c), time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 13:41, 4 April 2011 | 1,024 × 768 (108 KB) | Jml (talk | contribs) | Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 452(abc), 453(bc) and 454 (c), time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs. |