Jump to content

File:WF 2E03 mar23 2011-060b.jpg

From LabAdviser
Revision as of 12:41, 4 April 2011 by Jml (talk | contribs) (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 452(abc), 453(bc) and 454 (c), time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 768 pixels, file size: 108 KB, MIME type: image/jpeg)

Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 452(abc), 453(bc) and 454 (c), time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current12:41, 4 April 2011Thumbnail for version as of 12:41, 4 April 20111,024 × 768 (108 KB)Jml (talk | contribs)Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 452(abc), 453(bc) and 454 (c), time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs.

Metadata