File:WF 2E01 mar23 2011 090b.jpg
Appearance
Size of this preview: 800 × 600 pixels. Other resolution: 1,024 × 768 pixels.
Original file (1,024 × 768 pixels, file size: 95 KB, MIME type: image/jpeg)
Etching of nanostructures in Si using DRIE-Pegasus: nano1.3 recipe, Run ID 1856 (a) and 1857 (a+b), time 60 secs (a) and 120 secs (b), SF6 38, C4F8 52, 4mtorr, 600/40 coil/platen, -10 degs.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 15:01, 30 March 2011 | 1,024 × 768 (95 KB) | Jml (talk | contribs) | Etching of nanostructures in Si using DRIE-Pegasus: nano1.3 recipe, Run ID 1856 (a) and 1857 (a+b), time 60 secs (a) and 120 secs (b), SF6 38, C4F8 52, 4mtorr, 600/40 coil/platen, -10 degs. |